1. Resistant to moisture.
2. Chemical resistance.
3. Anti-biodegradation and animal destruction.
4. High temperature resistance.
5. UV resistance.
Iterm | Unit | Standard | Index | |||
HT500 | HT750 | HT1000 | ||||
Tensile Strength | Radial Direction | KN/M | ISO 10319-2015 | 85 | 130 | 220 |
Zonal Direction | KN/M | ISO 10319-2015 | 115 | 120 | 200 | |
Elongation at Break | Radial Direction | % | ISO 10319-2015 | 13 | 12 | 13 |
Zonal Direction | % | ISO 10319-2015 | 8 | 8 | 8 | |
Joint Tensile Strength | KN/M | ISO 10319-2015 | 90 | 100 | 170 | |
CBR | KN | GB/T14800-2010 | 9 | 15 | 20 | |
Dynamic Perforation | MM | GB/T17630-1998 | 8 | 10 | 80 | |
Effective Aperture(O90) | MM | GB/T14799-2005 | 0.45 | 0.4/0.28 | 0.45 | |
Permeability(Q50) | L/m2/s | GB/T15789-2005 | 35 | 14 | 18 | |
UV Resistance | % | ASTM D4355-2014 | 90 | 85 | 85 |
Within one month of the sludge volume can reduce more than 90%, basically for subsequent removal and handling easier.
Summer:86-18056028960
website:www.zhongloo.net