• Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill
  • Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill
  • Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill
  • Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill

Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner For Pond Liner And Landfill

 
1) Good physical and mechanic performance
2) High tearing resistance, strong deformation adaptability
3) Puncture-resisting, aging resisting, ultra-violet radiation, oil and salt, and corrosion resistance
4) Good adaptability to high and low temperature, non-toxicity, long service life
5) Good waterproof, drainage, anti-seepage and damp proof effects
6) Complete width and thickness specifications, low cost and easy installation.

Description:

Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner For Pond Liner And Landfill

 

 

Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill
 
1) Good physical and mechanic performance
2) High tearing resistance, strong deformation adaptability
3) Puncture-resisting, aging resisting, ultra-violet radiation, oil and salt, and corrosion resistance
4) Good adaptability to high and low temperature, non-toxicity, long service life
5) Good waterproof, drainage, anti-seepage and damp proof effects
6) Complete width and thickness specifications, low cost and easy installation.
Best Price 0.75mm Fish Farm Pond Liner 1.0mm Waterproof Geomembranas HDPE Liner for Pond Liner and Landfill
Geomembrane Technical Parameter (GB standard)
Spec
Properties
GMS0.5
GMS0.75
GMS1.0
GMS1.25
GMS1.5
GMS2.0
GMS2.5
Thickness
0.5mm
0.75mm
1.0mm
1.25mm
1.5mm
2.0mm
2.5mm
Tensile Properties
(each direction) (≥)
.yield strength
.break strength
.yield elongation
.break elongation


7KN/m
10KN/m
--
600%


10KN/m
15KN/m
--
600%


13KN/m
20KN/m
11%
600%


16KN/m
25KN/m
11%
600%


20KN/m
30KN/m
11%
600%


26KN/m
40KN/m
11%
600%


33KN/m
50KN/m
11%
600%
Density(≥)
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
Puncture Restistance (≥)
120N
180N
240N
300N
360N
480N
600N
Carbon Black Content
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
Carbon black Dispersion
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Tear Resistance (≥)
56N
84N
115N
140N
170N
2255N
280N
Oxidative Induction Time(OIT)
Standare OIT(≥)

60min.

60min.

60min.

60min.

60min.

60min.
 
60min.

Construction Method


1. The slope shall be laid in order from top to bottom. Don't pull it too tight.
2. Tow adjacent longitudinal joints should not be in a horizontal line, should bestaggered more than 1m each other.
3. Longitudinal joints should be more than 1.50m away from the dam foot and bending foot, and should be located on the plane.
4. When the slope is laid, the direction of spreading film should be basically parallel to the slope line.
5. The construction, first of all to use small diameter sand or clay levelingbase, and then laid the geomembrane. The geomembrane should not be stretched too tight, and the part of the soil bured at both ends is corrugated. A transitional layer of about 10cm is laid on the geomembrane with sand or clay.
Please contact me for more info today!
Anhui Zhonglu Engineering Materials Co., Ltd.
Summer@zhongloo.com
Summer Meng +86 18056028960